| Ningbo East Magnet Co.,Ltd |
| Factory Address: |
| Building No.D, ShiQi Industrial Park, NingBo,China |
Tel: +86-574-28828768(For export)
+86-574-88258767
+86 574 88272989 |
| Fax: +86 574 88258767 |
| Sales Manager :Mr. Kraft Xie |
| Email: sales@eastmagnets.com |
| Website: www.eastmagnets.com |
|
|
|
| |
| Product Show |
|
|
|
Sintered NdFeB Magnet
|
 |
Model No: |
Sintered Magnet |
Product Origin: |
China |
Brand Name: |
Ningbo East Magnets Co.,Ltd |
Payment Terms: |
FOB/CNF/CIF |
|
Delivery Lead Time: |
25-35days |
To purchase this Sintered Magnet or for more information,please E-mail us! |
 |
Or |
|
|
| |
| Detailed Product Description |
|
At present time, Sintered NdFeB is one of the strongest magnet materials available. It contributes to the development of many small and flat motors used in the high-tech industry. It¡¯s high residual induction (Br), high intrinsic Coercive force (Hcj) and high Energy Product (BH), makes it suitable for servo motors, disk brushless motors, stepping motors, IT industry, MRI, and audio products. For NdFeB,its surface is usually treatd with some special methods.The surface treatment method include Zine,Nickel,Tin,Silver,Gold plating,Phosphor and Spray Epoxy Resin etc Magnetic Properties of Sintered NdFeB Magnets
|
Grade |
Remanence |
Coercivity Force |
Intrinsic Coercive Force |
Max. Energy Product |
maximum Operating Temp. |
|
Br |
Hcb |
Hcj |
£¨ BH £© max |
|
mT |
kGs |
kA/m |
kOe |
kA/m |
kOe |
kJ/m3 |
MGOe |
|
N27 |
1030-1080 |
10.3-10.8 |
≥796 |
≥10.0 |
≥955 |
≥12 |
199-231 |
25-29 |
80 °C |
|
N30 |
1080-1130 |
10.8-11.3 |
≥796 |
≥10.0 |
≥955 |
≥12 |
223-247 |
28-31 |
80 °C |
|
N33 |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥955 |
≥12 |
247-271 |
31-34 |
80 °C |
|
N35 |
1170-1220 |
11.7-12.2 |
≥868 |
≥10.9 |
≥955 |
≥12 |
263-287 |
33-36 |
80 °C |
|
N38 |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥955 |
≥12 |
287-310 |
36-39 |
80 °C |
|
N40 |
1250-1280 |
12.5-12.8 |
≥907 |
≥11.4 |
≥955 |
≥12 |
302-326 |
38-41 |
80 °C |
|
N42 |
1280-1320 |
12.8-13.2 |
≥915 |
≥11.5 |
≥955 |
≥12 |
318-342 |
40-43 |
80 °C |
|
N45 |
1320-1380 |
13.2-13.8 |
≥923 |
≥11.6 |
≥955 |
≥12 |
342-366 |
43-46 |
80 °C |
|
N48 |
1380-1420 |
13.8-14.2 |
≥923 |
≥11.6 |
≥876 |
≥12 |
366-390 |
46-49 |
80 °C |
|
N50 |
1400-1450 |
14.0-14.5 |
≥796 |
≥10.0 |
≥876 |
≥11 |
382-406 |
48-51 |
60 °C |
|
N52 |
1430-1480 |
14.3-14.8 |
≥796 |
≥10.0 |
≥876 |
≥11 |
398-422 |
50-53 |
60 °C |
|
30M |
1080-1130 |
10.8-11.3 |
≥796 |
≥10.0 |
≥1114 |
≥14 |
223-247 |
28-31 |
100 °C |
|
33M |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥1114 |
≥14 |
247-263 |
31-33 |
100 °C |
|
35M |
1170-1220 |
11.7-12.2 |
≥868 |
≥10.9 |
≥1114 |
≥14 |
263-287 |
33-36 |
100 °C |
|
38M |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥1114 |
≥14 |
287-310 |
36-39 |
100 °C |
|
40M |
1250-1280 |
12.5-12.8 |
≥923 |
≥11.6 |
≥1114 |
≥14 |
302-326 |
38-41 |
100 °C |
|
42M |
1280-1320 |
12.8-13.2 |
≥955 |
≥12.0 |
≥1114 |
≥14 |
318-342 |
40-43 |
100 °C |
|
45M |
1320-1380 |
13.2-13.8 |
≥995 |
≥12.5 |
≥1114 |
≥14 |
342-366 |
43-46 |
100 °C |
|
48M |
1360-1430 |
13.6-14.3 |
≥1027 |
≥12.9 |
≥1114 |
≥14 |
366-390 |
46-49 |
100 °C |
|
50M |
1400-1450 |
14.0-14.5 |
≥1033 |
≥13.0 |
≥1114 |
≥14 |
382-406 |
48-51 |
100 °C |
|
30H |
1080-1130 |
10.8-11.3 |
≥796 |
≥10.0 |
≥1353 |
≥17 |
223-247 |
28-31 |
120 °C |
|
33H |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥1353 |
≥17 |
247-271 |
31-34 |
120 °C |
|
35H |
1170-1220 |
11.7-12.2 |
≥868 |
≥10.9 |
≥1353 |
≥17 |
263-287 |
33-36 |
120 °C |
|
38H |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥1353 |
≥17 |
287-310 |
36-39 |
120 °C |
|
40H |
1250-1280 |
12.5-12.8 |
≥923 |
≥11.6 |
≥1353 |
≥17 |
302-326 |
38-41 |
120 °C |
|
42H |
1280-1320 |
12.8-13.2 |
≥955 |
≥12.0 |
≥1353 |
≥17 |
318-342 |
40-43 |
120 °C |
|
45H |
1300-1360 |
13-13.6 |
≥963 |
≥12.1 |
≥1353 |
≥17 |
326-358 |
43-46 |
120 °C |
|
48H |
1370-1430 |
13.7-14.3 |
≥995 |
≥12.5 |
≥1353 |
≥17 |
366-390 |
46-49 |
120 °C |
|
30SH |
1080-1130 |
10.8-11.3 |
≥804 |
≥10.1 |
≥1592 |
≥20 |
223-247 |
28-31 |
150 °C |
|
33SH |
1130-1170 |
11.3-11.7 |
≥844 |
≥10.6 |
≥1592 |
≥20 |
247-271 |
31-34 |
150 °C |
|
35SH |
1170-1220 |
11.7-12.2 |
≥876 |
≥11.0 |
≥1592 |
≥20 |
263-287 |
33-36 |
150 °C |
|
38SH |
1220-1250 |
12.2-12.5 |
≥907 |
≥11.4 |
≥1592 |
≥20 |
287-310 |
36-39 |
150 °C |
|
40SH |
1240-1280 |
12.5-12.8 |
≥939 |
≥11.8 |
≥1592 |
≥20 |
302-326 |
38-41 |
150 °C | ,
|
42SH |
1280-1320 |
12.8-13.2 |
≥987 |
≥12.4 |
≥1592 |
≥20 |
318-342 |
40-43 |
150 °C |
|
45SH |
1320-1380 |
13.2-13.8 |
≥1003 |
≥12.6 |
≥1592 |
≥20 |
342-366 |
43-46 |
150 °C |
|
28UH |
1020-1080 |
10.2-10.8 |
≥764 |
≥9.6 |
≥1990 |
≥25 |
207-231 |
26-29 |
180 °C |
|
30UH |
1080-1130 |
10.8-11.3 |
≥812 |
≥10.2 |
≥1990 |
≥25 |
223-247 |
28-31 |
180 °C |
|
33UH |
1130-1170 |
11.3-11.7 |
≥852 |
≥10.7 |
≥1990 |
≥25 |
247-271 |
31-34 |
180 °C |
|
35UH |
1180-1220 |
11.8-12.2 |
≥860 |
≥10.8 |
≥1990 |
≥25 |
263-287 |
33-36 |
180 °C |
|
38UH |
1220-1250 |
12.2-12.5 |
≥876 |
≥11.0 |
≥1990 |
≥25 |
287-310 |
36-39 |
180 °C |
|
40UH |
1240-1280 |
12.5-12.8 |
≥899 |
≥11.3 |
≥1990 |
≥25 |
302-326 |
38-41 |
180 °C |
|
28EH |
1040-1090 |
10.4-10.9 |
≥780 |
≥9.8 |
≥2388 |
≥30 |
207-231 |
26-29 |
200 °C |
|
30EH |
1080-1130 |
10.8-11.3 |
≥812 |
≥10.2 |
≥2388 |
≥30 |
223-247 |
28-31 |
200 °C |
|
33EH |
1130-1170 |
11.3-11.7 |
≥836 |
≥10.5 |
≥2388 |
≥30 |
247-271 |
31-34 |
200 °C |
|
35EH |
1170-1220 |
11.7-12.2 |
≥876 |
≥11.0 |
≥2388 |
≥30 |
263-287 |
33-36 |
200 °C |
|
38EH |
1220-1250 |
12.2-12.5 |
≥899 |
≥11.3 |
≥2388 |
≥30 |
287-310 |
36-39 |
200 °C | Physical Properties of Sintered NdFeB Magnets
|
Temp.Coeff.of Br |
-0.11%/ °C |
Temp.Coeff.of Hc |
-0.60%/ °C |
|
Density |
7.3-7.5g/cm 3 |
Electrical Resistivity |
114 ¦Ì ¦¸ ..cm |
|
Vickers Hardness |
600Hv |
Flexural Resistivity |
25kg/mm |
|
Tensile Strength |
8.0Kg/mm2 |
Coeff. Of Thermal Expansion |
4X10 -6 / °C |
|
Specific Heat |
0.12Kcal/Kg |
Thermal Conductivity |
7.7kcal/[m.h. °C |
|
Young¡¯s Modulus |
1.6X10[11]N/m2 |
Rigidity |
0.64N/m2 |
|
Poisson¡¯s Ratio |
0.24 |
Compressibility |
9.8x10-12m2/N |
|
Curie Temperature |
310-340 °C |
|
| Process of Sintered NdFeB Magnets  |
|
|
|
|
|