AINiCo magnet is an alloy of aluminum-nickel-cobalt,has excellent temperature stability and corrosion resistance,it can be used in motor,sensor,separator,Loudspeaker and holding system etc....

Magnetic Properties of Sintered AlNiCo
|
Grade |
Remanence |
Coercivity Force |
Intrinsic Coercive Force |
Max. Energy Product |
max. continuous temperature |
Density |
Remarks |
|
Br |
Hcb |
Hcj |
( BH ) max |
|
|
|
mT |
kA/m |
kA/m |
kJ/m3 |
°C |
g/cm2 |
|
SAINiCo4/1 |
870-890 |
9-11 |
10-12 |
3.2-4.8 |
750 |
6.8 |
Isotropy |
|
SAINiCo8/5 |
530-620 |
45-50 |
47-52 |
8.5-9.5 |
750 |
6.8 |
|
SAINiCo10/5 |
630-700 |
48-56 |
50-58 |
9.5-11 |
780 |
6.8 |
|
SAINiCo12/5 |
700-750 |
50-56 |
53-58 |
11-13 |
800 |
7 |
|
SAINiCo14/5 |
730-800 |
47-50 |
50-53 |
13-15 |
790 |
7.1 |
|
SAINiCo14/6 |
620-810 |
56-64 |
58-66 |
14-16 |
790 |
7.1 |
|
SAINiCo14/8 |
550-610 |
75-88 |
80-92 |
14-16 |
850 |
7.1 |
|
SAINiCo18/10 |
570-620 |
92-100 |
99-107 |
16-19 |
860 |
7.2 |
|
SAINiCo35/5 |
1100-1200 |
48-52 |
50-54 |
35-39 |
850 |
7.2 |
Anisotropy |
|
SAINiCo29/6 |
970-1090 |
58-64 |
60-66 |
29-33 |
860 |
7.2 |
|
SAINiCo32/10 |
770-870 |
90-104 |
94-109 |
33-38 |
860 |
7.2 |
|
SAINiCo33/11 |
700-800 |
107-115 |
111-119 |
33-38 |
860 |
7.2 |
|
SAINiCo39/12 |
830-900 |
115-123 |
119-127 |
39-43 |
860 |
7.25 |
|
SAINiCo44/12 |
900-950 |
119-127 |
124-132 |
44-48 |
860 |
7.25 |
|
SAINiCo37/15 |
700-800 |
143-151 |
150-158 |
37-41 |
870 |
7.1 |
Process of Sintered AlNiCo Magnets